HIGH-KAPPA PULPING AND EXTENDED OXYGEN DELIGNIFICATION TO INCREASE YIELD, 2002 Kraft Pulp Yield Symposium
Please Note: This document will be available in PDF format in the "My Electronic Documents" link on the home page once your order has been completed. Please make sure you have the latest version of Acrobat Reader. Click on the Acrobat Reader icon to check for the latest version, it’s FREE. To print a hardcopy of a PDF file correctly you must have a postscript printer. If you are not sure if your printer is a postscript printer please refer to your owner’s manual.
The integration of extended oxygen delignification (EOD) into a bleached kraft southern pine mill is evaluated. ECF bleaching was used throughout to reach a target brightness of 83-86 % ISO. Comparisons with conventional kraft and conventional kraft/oxygen flowsheets were made. Production increase potential, environmental performance, impact on recovery, pulp strength and production unit costs were evaluated. The study utilized laboratory pulping, oxygen delignification and DEopD bleaching trials. Thelaboratory study provided input data for GEMS simulation of the entire pulp mill. On balance, kraft cooking to kappa 40, followed by (00) DEopD had the greatest productivity increase potential for both recovery boiler and digester limited mills. However, for a given mill’s product line, the economic optimum digester kappa number should be determined prior to the EOD stage(s) in each case.