KRAFT SWD YIELD : BREAK THE BARRIERS, 2002 Kraft Pulp Yield Anthology
Please Note: This document will be available in PDF format in the "My Electronic Documents" link on the home page once your order has been completed. Please make sure you have the latest version of Acrobat Reader. Click on the Acrobat Reader icon to check for the latest version, it’s FREE. To print a hardcopy of a PDF file correctly you must have a postscript printer. If you are not sure if your printer is a postscript printer please refer to your owner’s manual.
The improvement in Softwood (SWD) Full Bleached Kraft (FBK) Elemental Chlorine Free (ECF) yield when all known yield enhancements and fiber recovery methods are applied simultaneously in a 1,000 TPD example mill is examined. Wood preparation, chip properties, delignification methods, and bleaching to final product requirement are discussed and evaluated. Delignification processes include the current state of the art designs and novel modifications. A 5% yield increase above the base case is achievable. The manufactured costs are about $60/T below the base case. Some of the methods ate applicable to unbleached pulp, hardwood (HWD), and Totally Chlorine Free (TCF) methods. The design of the mill includes the potential to use whole log chipping.