Biphasic 1-butanol/water delignification of miscanthus for manufacturing papermaking pulp, TAPPI Journal August 2026

 


Application: This study provides a fundamental investigation of how butanol/water delignification conditions, especially additives, influence the resulting fiber and pulp properties. This information can be used as a benchmark to help assess the potential of butanol/water delignification against more common pulping chemistries.

TAPPI conference proceedings and presentations, technical papers, and publication articles provide technical and management data and solutions on topics covering the Pulp, Paper, Tissue, Corrugated Packaging, Flexible Packaging, Nanotechnology and Converting Industries.

Simply select the quantity, add to your cart and your conference paper, presentation or article will be available for immediate download.

Author: J. Gavin Gaynor, Dan Serrano, Lyndsay Clark, Gavin L. Gaynor and Lucian A. Lucia
Biphasic 1-butanol/water delignification of miscanthus for m
ABSTRACT: Miscanthus has emerged as a promising nonwoody fiber source for papermaking and fiber molding as the world has sought alternatives to wood-based products. A diverse range of chemistries have been explored at the laboratory scale to turn nonwoody biomass into fibers; however, few have been successful at pilot or commercial scales. An emerging organosolv delignification chemistry that has demonstrated previous technical success is butanol/water, having been shown to produce papers with similar properties to other, more conventional chemistries, but offering the benefit of a built-in sugar and lignin coproduct separation. While a range of fiber lengths were achieved (0.45•0.95 mm), addition of sodium hydroxide (NaOH) to the butanol/water delignification chemistry resulted in fiber lengths comparable to commercially available hardwood pulps (0.7•1.0 mm). Lignin concentration was reduced from 19.1 wt% in the raw miscanthus to under 3.5 wt% for most trials. The lowest lignin concentration (2.5 wt%) was achieved at 180°C for 180 min with 50:50 butanol:water and 2 wt% acetic acid. Yet, the high severity of this condition (and similar ones) resulted in a significant truncation of fiber length, which is detrimental for papermaking applications. The highest quality pulp for papermaking was generated at 180°C for 180 min with 50:50 butanol:water and 10 wt% NaOH. This pulp had one of the longest fiber lengths, the highest brightness, and the highest hemicellulose concentration. Thus, butanol/water delignification, especially with NaOH addition, resulted in the successful production of cellulose-rich pulps that have potential in commercial papermaking and fiber molding applications.
0.00

New Releases

TAPPI PRESS Catalog eBook 2026


Experience the Power of Publications in 2026


Open


 

Kraft Recovery Boilers, Third Edition  


Sponsored by the Recovery Boiler Program R&D Subcommittee of the American Forest & Paper Association (AF&PA) and published by TAPPI Press.


Purchase


 

Handbook For Pulp and Paper Technologists (The SMOOK Book), Fourth Edition

The best-selling text to introduce the entire technology of pulp and paper manufacture.

Purchase

 

Guidelines for Safe Assessment and Operation of Yankee Dryers  


A project of the Yankee Dryer Safety & Reliability Committee.

Purchase

 

Check our newest additions.


TAPPI Press offers some of the most in-depth resources and references for the forest products and related industries. 

See More

   
 

Available for Purchase – Conference Proceedings


TAPPI maintains a record of key conference papers, presentations, and other conference publications, available for purchase in a variety of formats.

See More